Quench Polish Quench - Process

Process

The process starts with a standard salt bath nitrocarburizing cycle, which produces a layer of ε iron nitride. Next, the workpiece is mechanically polished; typical polishing processes include vibratory finishing, lapping, and centerless grinding. Finally, the workpiece is re-immersed into the salt quench bath for 20 to 30 minutes, rinsed, and oil dipped. This last step optimizes the corrosion resistance by creating a 3 to 4 micrometre thick layer of iron oxide. It also gives the workpiece a black finish.

Read more about this topic:  Quench Polish Quench

Famous quotes containing the word process:

    “Because her instinct has told her, or because she has been reliably informed, the faded virgin knows that the supreme joys are not for her; she knows by a process of the intellect; but she can feel her deprivation no more than the young mother can feel the hardship of the virgin’s lot.”
    —Arnold Bennett (1867–1931)

    “We tend to be so bombarded with information, and we move so quickly, that there’s a tendency to treat everything on the surface level and process things quickly. This is antithetical to the kind of openness and perception you have to have to be receptive to poetry. ... poetry seems to exist in a parallel universe outside daily life in America.”
    —Rita Dove (b. 1952)

    “There was only one catch and that was Catch-22, which specified that a concern for one’s own safety in the face of dangers that were real and immediate was the process of a rational mind.... Orr would be crazy to fly more missions and sane if he didn’t, but if he was sane he had to fly them. If he flew them he was crazy and didn’t have to; but if he didn’t want to he was sane and had to.”
    —Joseph Heller (b. 1923)